FIGURE 6 Plasma sprayed liner from unlubricated wear test.

Counterface = Cr203 plasma sprayed ring. Cameron Plint. 400 C. 1 hour test. 250 N normal load, 5 mm stroke reciprocating at 10 Hz. Magnification X1000

FIGURE 7 cr203 Plasma sprayed liner from lubricated wear test

Polyester Counterface =

based Cr203 plasma synthetic sprayed ring, lubricant Cameron Plint, 420

C. 3 hour test. 250 N normal load. 5 mm stroke.

reciprocating at 10 Hz.

Magnification X1000

TABLE 1 Summary of Wear Test Equipment TESTER

Cameron Plint TE77

Falex #9

Hohman A9

Falex #1